soheilmd
Active Member
I tried to print a kraton bumper today with a new rol nylon.
The damn thing just starts warping en after that it starts to come lose.
And now the facts:
Creality K1 260C and bed started from 60C and bumped up by 10C every try until reached 100C
Its a new rol from brand overture from amazon.
I tried a clean bed, bed with painters tape, original glue stick that came with the printer, even glue stick on painters tape!
Increased the brim to 20 lines!
Just after 15 a 16 layers en corners become warped en causing the nozzle hiting them or just come lose.
And what i noticed was that the printed items break easy. Much easier than ABS+. There is no flex just snaps.
Any tip is highly appreciated.
The damn thing just starts warping en after that it starts to come lose.
And now the facts:
Creality K1 260C and bed started from 60C and bumped up by 10C every try until reached 100C
Its a new rol from brand overture from amazon.
I tried a clean bed, bed with painters tape, original glue stick that came with the printer, even glue stick on painters tape!
Increased the brim to 20 lines!
Just after 15 a 16 layers en corners become warped en causing the nozzle hiting them or just come lose.
And what i noticed was that the printed items break easy. Much easier than ABS+. There is no flex just snaps.
Any tip is highly appreciated.
Last edited: